Pack Size, ml | REF | Price, € |
---|---|---|
5 | MB-E1-5 | On request |
10 | MB-E1-10 | On request |
50 | MB-E1-50 | On request |
100 | MB-E1-100 | On request |
Specifications | |
---|---|
Concentration | 10 mg/ml |
Composition | γ˗Fe2O3‒SiO2‒poly(GMA-co-MBA) |
Surface functional groups | Epoxy |
Concentration of funcitonal groups | 0.6 mmol/g |
Average particle size | 20-40 μm |
Sedimentation stability | 2‒3 min |
Time of full magnetic separation | < 1 min* |
Magnetisation type | Superparamagnetic |
Magnetisation value | ~40 emu/g |
Storage conditions | 2‒8 ºC |
Transportation conditions | 2‒25 ºC |
Shelf life | 12 months |
*Depends on the isolation conditions. Magnetic rack is recommended |